Sigma phase occurs in Ferritic, martensitic, austenitic and duplex stainless steels when exposed to temperatures in the range of _____.
A) 537º C - 954º C
B) 621º C - 926º C
C) 676º C - 760º C
D) 584º C - 840º C
Correct Answer:
Verified
Q292: Titanium Hydriding damage occurs primarily in sour
Q293: Corrosion by HF (Hydrofluoric) acid can result
Q294: _ is a selective corrosion mechanism in
Q295: Areas of vulnerability in sulfuric acid Alkylation
Q296: A form of corrosion that can occur
Q298: _ is often found in piping and
Q299: Caustic is sometimes added to process streams
Q300: Which of the following materials are subject
Q301: With 885º F embrittlement, increasing amounts of
Q302: The creep threshold temperature for carbon steel