Carbide precipitation occurs in some stainless steels when they are kept at a temperature between ____ degrees Fahrenheit for a long period of time.
A) 800 and 1500
B) 1000 and 2100
C) 1500 and 2100
D) 1700 and 2100
Correct Answer:
Verified
Q5: In the GTAW process, contamination left on
Q11: Using a _ arc current setting with
Q16: When might the GTAW process be used
Q21: During the manufacturing process, sometimes pockets of
Q26: Why would a welder stick the end
Q27: When tungsten touches the molten weld pool,
Q29: Failure to remove tungsten contamination properly will
Q33: What can cause porosity (tiny bubbles) to
Q34: The greater the contamination of a stainless
Q39: The most common types of contaminants are