Surface cracks can be located by using either a liquid penetrant or a _____ inspection process.
A) grinding
B) slag removal
C) magnetic particle
D) preheating
Correct Answer:
Verified
Q6: The pipe size, schedule, and _ will
Q7: _ are pockets of material within a
Q8: _ uses a solution that is applied
Q9: When removing slag, eliminate the _ pieces
Q10: Insufficient _ can result in rapid cooling
Q12: When repairing a weld, use a(n)_ or
Q13: _ are typically encountered with processes that
Q14: A(n)_ grinder is easier to control and
Q15: Why is it important to grind the
Q16: Incomplete joint penetration is a discontinuity associated