If weld repairs are required, the effects of temper embrittlement can be temporarily reversed (de-embrittled) by heating at ______ for 2 hours per inch of thickness and rapidly cooling to room temperature.
A) 1000º F
B) 1150º F
C) 1200º F
D) 1250º F