SSC is a form of ________ stress corrosion cracking.
A) Hydrogen
B) Caustic
C) Polythionic
D) Alkaline
Correct Answer:
Verified
Q351: With sour water corrosion, at a given
Q352: Ammonium chloride salts are hydroscopic and readily
Q353: Cracking susceptibility increases with _ pH and
Q354: Blistering, HIC, SOHIC and SSC damage can
Q355: Amine cracking is a form of _
Q357: Galvanized steel components should not be welded
Q358: The major factors affecting high temperature sulfidation
Q359: Blistering, HIC and SOHIC have been found
Q360: _ of the amine system is the
Q361: Susceptibility to sulfidation is determined by the