What can cause porosity (tiny bubbles) to form on some welds on mild steel?
A) A chemical reaction between the filler metal and the mild steel.
B) Using the wrong type of tungsten electrode.
C) Small pockets of CO2 trapped inside of the steel during manufacturing.
D) Too much heat and the metal begins to boil.
Correct Answer:
Verified
Q5: In the GTAW process, contamination left on
Q11: Using a _ arc current setting with
Q16: When might the GTAW process be used
Q21: During the manufacturing process, sometimes pockets of
Q27: When tungsten touches the molten weld pool,
Q28: Why is it important to keep your
Q29: Failure to remove tungsten contamination properly will
Q29: How can a welder improve the shielding
Q34: The greater the contamination of a stainless
Q35: Carbide precipitation occurs in some stainless steels
Unlock this Answer For Free Now!
View this answer and more for free by performing one of the following actions
Scan the QR code to install the App and get 2 free unlocks
Unlock quizzes for free by uploading documents